Additive manufactured medical implants to enter mainstream

Back to Media and Events 2013-07-creepimage-inspecting-creep-damage-in-critical-power-plant-components 2016-09-cutting-edge-technology-for-nuclear-decommissioning A career in welding inspection Additive manufactured medical implants to enter mainstream Additive Manufacturing UK Strategy update available for download Advanced electron beam facilities meet advanced industrial challenges Advanced ultrasonic full matrix capture inspection software launched Armourers & Brasiers' awards open for entries Art exhibition leads to new method of laser metal deposition Asbestos detection made easier and more reliable ASME issues White Paper on auditing of welding Audit shows TWI as integral to innovation Aviation Industry Corporation of China collaborates with TWI BeamAssure™ – electron beam welding quality assurance tool Best practice for nuclear construction industry welding BS 7910:2013 - Assessing flaws in metallic structures Call for papers: 12th International FSW Symposium CII and TWI awareness seminar in composites technology Coatings and surface engineering: addressing the needs of industry Combatting ice and erosion in extreme low temperatures - EIROS Combining Cathodic Protection with Aluminium Coatings CROWN project commended for offshore wind corrosion work Depositing silicon carbide coatings by thermal spraying Digital Twin Technology to monitor offshore assets Digital twin technology wins environmental business award Dr Melissa Riley presents paper at international conference Dr Melissa Riley represents TWI at international conference eLearning package for CSWIP 3.1 Welding Inspector launched Entry is now open for SkillWeld 2016 Extending Aircraft Life Using Cold Spray Technology Fibre delivered laser beam cutting optimisation Friction stir welding – joining the future of industry Friction stir welding and Japanese jewellery Government funds £10 million technology hub in Teesside Has your PCN NDT Certification been voided? TWI Can Help… Her Royal Highness The Princess Royal opens new laboratories at TWI High-pressure hydrogen testing at TWI Ice-repellant coating for aerospace and energy industries Industry benefits of composites microwave processing Innovation Centres at TWI deliver progress for industry INTRAPID produces rapid in-line laser AM inspection systems Introducing the TWI Virtual Academy: studying on your own terms Investigating geothermal coatings for the future of renewable energy Laser scanner improves TWI weld analysis services for Members Lasers for decommissioning: the story so far Lifting the lid on innovation: exploratory projects at TWI Lord Heseltine opens new TWI technology and training centre Meeting reinvigorates Welding Institute's Liverpool branch Mike Russell appointed as TWI Operations Director 'Mind the doors' – New project investigates train door failure Mobile electron beam welds for fabricating large structures ModuLase - combining laser processes for the future of manufacturing MoU between ALFED and TWI enhances collaboration Nanosecond pulsed laser expands opportunities for project work NDT Voiding of PCN certification from NDT International New benefit for TWI Members: free access to Welding Abstracts journal New building to house TWI's structural integrity expertise New centre for Advanced Manufacturing Technologies launched New eBooks added for Professional and Industrial Members New facility for testing the barrier performance of polymers New Granta Centre manager guarantees premier conferencing New home and new capabilities for TWI in Middlesbrough New manufacturing process supports Hayter's winning position New sensor technology for safe shale gas extraction funded New TWI article breaks down the changes to ISO 15614-1 New ultrasonic testing courses from the TWI Virtual Academy New welding apprenticeship standards receive government approval Novel solution for submersible pumps in oil and gas industry Open Day sparks the start of a new era of research for TWI Pioneering tests being conducted on bespoke TWI rig Plant Inspection training meets need for competent workers Plastics welding experts answer your questions at Aquaculture UK 2014 Progressing graphene as a supercritical fluid barrier Project investigates Powder Metallurgy for astrospace use Purpose-built pressure testing facility opens for business at TWI Purpose-built pressure testing facility to be constructed at TWI Registration opens for TWI BS EN ISO 15614-1 (2017) training RJD Engineering gains Factory Production Control system Certification Rolls-Royce's Martin Boyd discusses the benefits of becoming an IEng Showing expertise in corrosion safety, investigation and assessment Simulating real-world conditions for oil and gas research Skills Development Fund Scheme provides extra TWI courses SkillWeld medallist goes on to take gold at EuroSkills 2016 SOCAR and TWI celebrate new competence training partnership Success for TWI's first blended learning course candidates Successful engineers graduate from EWF/IIW Diploma in Welding 'SUPERSLAB' to meet thicker high-strength steels challenge SurFlow: secure, robust, integrated data transfer through composites Symposium highlights developments in linear friction welding Taking the next step as a CSWIP Welding Inspector Tate Modern use solvent technology for art restoration Teletest business transfers to Eddyfi Technologies The 50-year view of fracture The Transport Systems Catapult and TWI Announce Partnership The Welding Institute Annual Awards and Dinner 2017 The Welding Institute Awards 2018 – Applied Technology Award The Welding Institute promoting career development at NECR exhibition True Stress-True Strain Tensile Testing to Failure TWI and Lloyd's Register launch Fullagar Technologies initiative TWI and Lloyd's Register projects advance take-up of AM TWI celebrates National Women in Engineering Day TWI CEO Christoph Wiesner awarded OBE TWI combines heritage with innovation for the Morgan Motor Company TWI commence 'SubSeaLase' decommissioning project TWI delivers plastics welding training course to Fusion Marine TWI develops essential metallography training to ensure best practice TWI enters research centre agreement with AECC BIAM, China TWI helping UK businesses to 'Access India' TWI helps bring Philips Avent's thermoplastic nebulizer to market TWI helps Engineering College meet industry demand for staff TWI holds successful cold spray technology course TWI hosts graduation ceremony for EWF/IIW Diploma engineers TWI joins 'Integral' nuclear waste project TWI lands NDA innovation award for nuclear decommissioning TWI launches course for advanced digital radiography TWI pioneers 'invisible weld' process TWI Pioneers New Dissimilar Weld for European Space Agency TWI rewards outstanding undergraduate engineering projects TWI signs Memorandum of Understanding with Saudi Aramco TWI Supports Underwater Laser Cutting Project TWI Technology Fellow given Visiting Professorship at LSBU TWI Training success story - Vera Dragoi TWI wins RIBA Awards TWI working to progress composites in the automotive industry TWI's Dr Philippa Moore: A role model for female engineers TWI's Dr Shiladitya Paul called as guest editor of Coatings journal Ultrasonic imaging climbing robot passes field trials Update on CPD for Welding Institute Professional Members Vince Cable India visit promotes UK business successes Welding Institute Annual Awards 2018 Welding Institute's latest Engineering Council registrants Welding the unweldable: TWI friction stir welds ODS steel WindTwin project to revolutionise wind turbine technology Workshop to address dissimilar materials joining challenge World's largest linear friction welded component produced World's most precise weld made at TWI
 
05 February 2016
Examples of the lattice structures created under the project
Examples of the lattice structures created under the project. The structure on the left is randomised, the one on the right uniform.

Hip and spinal joint replacement patients could soon be receiving individualised, metal 3D-printed implants, thanks to a pioneering project from an industry partnership.

TWI has collaborated with Metalysis, the metal powder technology company, to demonstrate the feasibility of its tantalum powder in metal additive layer manufacturing for biomedical applications such as patient-bespoke hip joints. The project successfully produced both uniform and randomised tantalum lattice structures that are bio-inert, replicate the structural stiffness of bone and allow for extensive integration with bone cells, so that the new joint is readily accepted by the body.

Metalysis has developed a process that produces metal powders directly from their respective oxides in just a single step, drastically lowering the environmental impact of its manufacture. The innovative process is not only cost-competitive, but also produces perfectly spherical metal powders of uniform size so that when used in metal additive manufacturing, the end product is structurally consistent and allows for an improvement  on the as-built surface finish. This study has proved that the properties (ie durability and inertness) of this highly versatile metal are retained through the production process. This is due to the quality of Metalysis’ powders which allows the 3D printer to lay down the metal, forming a lattice structure, with consistent strength and density.

To date, most additive manufacturing technologies have focused on the use of commodity plastics, because  powdered metals, until now, have proved too expensive to be widely used for this process. Now, Metalysis’ high-quality metal powder, combined with TWI’s expertise, has demonstrated the significant potential of creating lattice structures using a specific metal additive manufacturing technique – selective laser melting (SLM) – for use in hip joints, implants and other new biomedical products that will both benefit patient wellbeing and bring cost savings to the wider market. TWI has a history of bringing advances to the medical industry, and this study shows that Metalysis’ metals can be used to manufacture prototypes of  the highest levels of quality by exploiting SLM additive manufacturing technology.

Metalysis is spearheading a revolution in the production of high-quality metals including tantalum and titanium. Its patented process replaces the outdated, extremely expensive and highly toxic Kroll or Hunter process which has been used for the past 70 years. Up until now, the inefficiency and expense of this process has made titanium and tantalum prohibitively expensive. Since the launch of its commercial plant in 2015, Metalysis has been supplying tantalum powder to clients around the world, working in collaboration with LPW Technology to serve its additive manufacturing customers.

A TWI spokesman said: ‘We have already seen the great success Metalysis has had printing automotive parts. Our analysis suggests these metals are incredibly versatile and highly suited to the medical industry. Metal 3D-printed hip replacements could be a huge step forward, allowing patients to have a tailor-made joint by scanning their other hip and matching it with a metal 3D-printed replacement, rather than being restricted to the choice of standard sizes now available.’

Dion Vaughan, chief executive of Metalysis, said: ‘It is tremendous to be partnering with TWI, a company that has so much knowledge in the manufacturing and medical industries. TWI has great expertise, particularly in the use of lasers in additive manufacturing, which we hope will help to bring individual joint replacements into the mainstream of mass manufacture.’

For more information on this project and TWI's additive manufacturing capability, contact us.