Back to Media and Events 2013-07-creepimage-inspecting-creep-damage-in-critical-power-plant-components 2016-09-cutting-edge-technology-for-nuclear-decommissioning A career in welding inspection Additive manufactured medical implants to enter mainstream Additive Manufacturing UK Strategy update available for download Advanced electron beam facilities meet advanced industrial challenges Advanced ultrasonic full matrix capture inspection software launched Armourers & Brasiers' awards open for entries Art exhibition leads to new method of laser metal deposition Asbestos detection made easier and more reliable ASME issues White Paper on auditing of welding Audit shows TWI as integral to innovation Aviation Industry Corporation of China collaborates with TWI BeamAssure™ – electron beam welding quality assurance tool Best practice for nuclear construction industry welding BS 7910:2013 - Assessing flaws in metallic structures Call for papers: 12th International FSW Symposium CII and TWI awareness seminar in composites technology Coatings and surface engineering: addressing the needs of industry Combatting ice and erosion in extreme low temperatures - EIROS Combining Cathodic Protection with Aluminium Coatings CROWN project commended for offshore wind corrosion work Depositing silicon carbide coatings by thermal spraying Digital Twin Technology to monitor offshore assets Digital twin technology wins environmental business award Dr Melissa Riley presents paper at international conference Dr Melissa Riley represents TWI at international conference eLearning package for CSWIP 3.1 Welding Inspector launched Entry is now open for SkillWeld 2016 Extending Aircraft Life Using Cold Spray Technology Fibre delivered laser beam cutting optimisation Friction stir welding – joining the future of industry Friction stir welding and Japanese jewellery Government funds £10 million technology hub in Teesside Has your PCN NDT Certification been voided? TWI Can Help… Her Royal Highness The Princess Royal opens new laboratories at TWI High-pressure hydrogen testing at TWI Ice-repellant coating for aerospace and energy industries Industry benefits of composites microwave processing Innovation Centres at TWI deliver progress for industry INTRAPID produces rapid in-line laser AM inspection systems Introducing the TWI Virtual Academy: studying on your own terms Investigating geothermal coatings for the future of renewable energy Laser scanner improves TWI weld analysis services for Members Lasers for decommissioning: the story so far Lifting the lid on innovation: exploratory projects at TWI Lord Heseltine opens new TWI technology and training centre Meeting reinvigorates Welding Institute's Liverpool branch Mike Russell appointed as TWI Operations Director 'Mind the doors' – New project investigates train door failure Mobile electron beam welds for fabricating large structures ModuLase - combining laser processes for the future of manufacturing MoU between ALFED and TWI enhances collaboration Nanosecond pulsed laser expands opportunities for project work NDT Voiding of PCN certification from NDT International New benefit for TWI Members: free access to Welding Abstracts journal New building to house TWI's structural integrity expertise New centre for Advanced Manufacturing Technologies launched New eBooks added for Professional and Industrial Members New facility for testing the barrier performance of polymers New Granta Centre manager guarantees premier conferencing New home and new capabilities for TWI in Middlesbrough New manufacturing process supports Hayter's winning position New sensor technology for safe shale gas extraction funded New TWI article breaks down the changes to ISO 15614-1 New ultrasonic testing courses from the TWI Virtual Academy New welding apprenticeship standards receive government approval Novel solution for submersible pumps in oil and gas industry Open Day sparks the start of a new era of research for TWI Pioneering tests being conducted on bespoke TWI rig Plant Inspection training meets need for competent workers Plastics welding experts answer your questions at Aquaculture UK 2014 Progressing graphene as a supercritical fluid barrier Project investigates Powder Metallurgy for astrospace use Purpose-built pressure testing facility opens for business at TWI Purpose-built pressure testing facility to be constructed at TWI Registration opens for TWI BS EN ISO 15614-1 (2017) training RJD Engineering gains Factory Production Control system Certification Rolls-Royce's Martin Boyd discusses the benefits of becoming an IEng Showing expertise in corrosion safety, investigation and assessment Simulating real-world conditions for oil and gas research Skills Development Fund Scheme provides extra TWI courses SkillWeld medallist goes on to take gold at EuroSkills 2016 SOCAR and TWI celebrate new competence training partnership Success for TWI's first blended learning course candidates Successful engineers graduate from EWF/IIW Diploma in Welding 'SUPERSLAB' to meet thicker high-strength steels challenge SurFlow: secure, robust, integrated data transfer through composites Symposium highlights developments in linear friction welding Taking the next step as a CSWIP Welding Inspector Tate Modern use solvent technology for art restoration Teletest business transfers to Eddyfi Technologies The 50-year view of fracture The Transport Systems Catapult and TWI Announce Partnership The Welding Institute Annual Awards and Dinner 2017 The Welding Institute Awards 2018 – Applied Technology Award The Welding Institute promoting career development at NECR exhibition True Stress-True Strain Tensile Testing to Failure TWI and Lloyd's Register launch Fullagar Technologies initiative TWI and Lloyd's Register projects advance take-up of AM TWI celebrates National Women in Engineering Day TWI CEO Christoph Wiesner awarded OBE TWI combines heritage with innovation for the Morgan Motor Company TWI commence 'SubSeaLase' decommissioning project TWI delivers plastics welding training course to Fusion Marine TWI develops essential metallography training to ensure best practice TWI enters research centre agreement with AECC BIAM, China TWI helping UK businesses to 'Access India' TWI helps bring Philips Avent's thermoplastic nebulizer to market TWI helps Engineering College meet industry demand for staff TWI holds successful cold spray technology course TWI hosts graduation ceremony for EWF/IIW Diploma engineers TWI joins 'Integral' nuclear waste project TWI lands NDA innovation award for nuclear decommissioning TWI launches course for advanced digital radiography TWI pioneers 'invisible weld' process TWI Pioneers New Dissimilar Weld for European Space Agency TWI rewards outstanding undergraduate engineering projects TWI signs Memorandum of Understanding with Saudi Aramco TWI Supports Underwater Laser Cutting Project TWI Technology Fellow given Visiting Professorship at LSBU TWI Training success story - Vera Dragoi TWI wins RIBA Awards TWI working to progress composites in the automotive industry TWI's Dr Philippa Moore: A role model for female engineers TWI's Dr Shiladitya Paul called as guest editor of Coatings journal Ultrasonic imaging climbing robot passes field trials Update on CPD for Welding Institute Professional Members Vince Cable India visit promotes UK business successes Welding Institute Annual Awards 2018 Welding Institute's latest Engineering Council registrants Welding the unweldable: TWI friction stir welds ODS steel WindTwin project to revolutionise wind turbine technology Workshop to address dissimilar materials joining challenge World's largest linear friction welded component produced World's most precise weld made at TWI
 
16 December 2015

TWI has acquired a new weld-scanning laser tool which is able to quickly measure the external properties of welds.

The latest addition to TWI's technology portfolio is a WiKi-SCANT weld inspection tool, manufactured by Canadian laser specialists Servo-Robot. The acquisition is already manifesting an improved service to Member companies, and has the potential to reduce the duration and cost of projects requiring the analysis of weld properties.

WiKi-SCAN uses a laser and advanced calibration to take weld root mismatch measurements, along with other important parameters including weld bead width or leg length and weld bead height. The measured weld profile can also be used to measure weld toe angle.

The external properties of a weld can control aspects of the weld's mechanical properties; the size of a weld affects its load-carrying capacity; and the weld bead profile, weld root mismatch (otherwise known as 'hi-lo') and shape of the weld bead at the weld toe can have an influence on fatigue strength.

Taking manual measurements of weld root mismatch can be time consuming, and once the measurement has been taken and recorded, there is no permanent record of what has been measured.

Weld bead toe angle is usually obtained by cutting a slice from the weld, mounting and polishing the slice and then photographing it. This destroys the area of interest, takes time and can add significant cost to projects if multiple measurements are required.

WiKi-SCAN records weld profile information and takes an accompanying photograph of the weld at each measurement position. It can be used to measure weld profiles on many types of weld, including butt, girth and fillet, and measurements can be taken at specific locations or in 'continuous mode', which records a profile and photograph at a user-specified intervals along the weld length.

The quick and user-friendly method provides TWI Members with a permanent record of the weld profile and appearance of the weld at the measurement locations.

TWI has carried out trials and found that the measurements are repeatable and correlate with other methods of taking these measurements within acceptable limits.

 

To find out how we can use WiKi-SCAN to help your business, contact us.

Photograph of a girth weld root bead taken using WiKi-SCAN at the measurement location
Photograph of a girth weld root bead taken using WiKi-SCAN at the measurement location
Weld profile produced from WiKi-SCAN, which can be used to obtain information such as weld toe angle without the need for destructive sectioning
Weld profile produced from WiKi-SCAN, which can be used to obtain information such as weld toe angle without the need for destructive sectioning