Cold spray additive manufacturing (CSAM) produces near-net-shape metal components by depositing powder particles in the solid-state, without melting the feedstock. Combining high deposition rates with low heat input, the process offers a route to manufacturing and repairing components while minimising oxidation, thermal distortion and heat-affected zones.
Having found early applications in coating and repair, cold spray is now increasingly being explored for additive manufacturing, including multi-material deposition and functionally graded structures.
With more than two decades of experience in cold spray research and development, TWI supports Industrial Members and publicly funded programmes in advancing this technology through materials research, process development, prototype-scale manufacturing and process qualification. Our work spans a range of industrial sectors, including aerospace, space, defence and energy.
How does Cold Spray Additive Manufacturing Work?
A preheated, high-pressure gas stream accelerates fine powder particles to supersonic velocities before directing them onto a substrate material. On impact, the particles undergo severe plastic deformation, forming a bond with the substrate and previously deposited material without melting. Successive layers of deposited particles are built up layer by layer to produce a component with the desired geometry.
In contrast to thermal spray processes or fusion-based additive manufacturing processes such as electron beam / selective laser melting and laser metal deposition, cold spray does not rely on melting and solidification of the feedstock materials to form a deposit. This reduces the thermal input during processing and helps minimise associated microstructural changes. Where required, post-deposition thermal treatments can be applied to modify the microstructure and improve mechanical properties, with the treatment selected according to the material and application.
The deposition process is influenced by powder characteristics, particle velocity, gas conditions and the interaction between the deposited material and substrate. These parameters are important in controlling deposit quality, bonding and the overall performance of the manufactured component.
Watch our video: Cold Spray Additive Manufacturing of Hollow Cylinder.
Advantages of Cold Spray Additive Manufacturing
- Solid-state processing: Deposition without melting limits thermal effects, helping to preserve the properties of temperature- and oxidation-sensitive materials.
- High deposition rates: Rapid material build-up supports efficient near-net-shape manufacturing and offers the potential to reduce material waste and machining requirements.
- Multi-material capability: The ability to co-deposit different powders enables the development of metal-matrix composites and functionally graded materials, allowing material composition and properties to be tailored to specific applications.
- Scalability: Robotic systems and large-scale cold spray facilities support process development from initial material trials through to prototype component manufacture.
Cold Spray Additive Manufacturing at TWI
TWI combines specialist cold spray facilities with complementary expertise in numerical modelling, powder metallurgy, thermal treatments, microstructural characterisation, non-destructive evaluation and mechanical testing. Together, these capabilities support the development, optimisation and assessment of cold spray materials and processes for additive manufacturing applications. Our facilities include:
- Titomic TKF-1000 high-pressure cold spray cell: Designed for additive manufacturing and production, the TKF-1000 features a dual powder feeder that enables the co-deposition of materials to produce metal-matrix composites and functionally graded structures. The system also offers nitrogen and helium process-gas capability.
- Impact Innovations 5/11 high-pressure cold spray system: Installed in our large-scale spray facility, this system is mounted on a six-axis robot and linear track. Offline toolpath programming supports the development of complex deposition strategies, while laser-assisted cold spray capability enables the investigation of challenging materials and deposition conditions.
- Titomic D523 low-pressure cold spray system: Our portable D523 system provides additional flexibility for low-pressure cold spray applications and development activities.
Through collaborative research and application-specific development, TWI supports Industrial Members in assessing the suitability of CSAM for specific applications. This includes material selection, feedstock assessment, deposition trials, parameter optimisation, toolpath development and the evaluation of post-deposition thermal treatments. Our complementary expertise in characterisation, non-destructive evaluation and mechanical testing supports the assessment of deposit properties and structural integrity, as well as process evaluation and qualification. TWI also offers bespoke cold spray training covering the underlying process principles and applications in additive manufacturing, coating and repair.

Figure 1: Free-standing cylindrical feature manufactured from 316L stainless steel using cold spray additive manufacturing.