Mechanical Fastening of Steel to Aluminium for Automotive

Back to Core Research Programme 33632-2021-review-of-materials-am-and-nde-considerations-for-functionally-graded-materials 34236-2023-literature-review-on-the-potential-use-of-non-destructive-testing-techniques-for-residual-stress-measurement 34241-2023-artificial-intelligence-for-ndt-scanning-of-unknown-geometries-using-collaborative-robots 34459-2022-friction-stir-welding-of-pressure-vessel-liners-for-the-storage-and-transportation-of-hydrogen 34727-2023-techniques-for-high-temperature-ultrasonic-inspection-of-arc-welding-state-of-the-art-review 34793-2023-update-on-literature-reviews-for-wire-fed-additive-manufacturing 34847-2023-Literature-review-on-crack-length-measurement-techniques-on-environmental-fracture-toughness-tests 35268-2024-Literature-review-on-dual-sensing-applications-for-SHM-of-pipelines 32221-2020-hybrid-composite-to-metal-joining 32893-2020-mechanical-fastener-coatings-for-corrosion-protection 33557-2020-extreme-high-speed-laser-application-ehla-coatings 33557-2020-extreme-high-speed-laser-application-ehla-coatings 33557-2020-extreme-high-speed-laser-application-ehla-coatings 33557-2020-review-of-electric-vehicle-battery-joining-methods-and-testing 34250-2022-thermoplastic-materials-compatibility-for-hydrogen-service A Review of High Power, In-Vacuum and Narrow Gap Laser Welding Processes for Thick Section Welding A Review of High Productivity Additive Manufacture Using a Hybrid Laser-Arc Deposition (HLAD) Process A Review of Micro Welding with Fibre and Disc Continuous-Wave Laser Sources A Review of Residual Stress Measurement Techniques Used for Components Produced Using the Selective Laser Melting Process A Review of the Machine GTAW Ambient Temperature Temper Bead Repair Technique for Nuclear Power Plant Components A Review of Weld Repairs of Mar-M247 and Similar Alloys Applications, Modelling and Manufacturing Processes for Perforated Composites - Literature Review Butt Fusion Welding Procedures and Test Methods Used for PE Pipes Duplex Stainless Steel Welding – A Review of Current Practices Elastic Follow-Up in the Context of Fracture Assessment Flaw Sizing Techniques Using Guided Waves Flaw Sizing Techniques Using Guided Waves Flaw Sizing Techniques Using Guided Waves In-Bore Multi-Positional Laser Welding In-Process Monitoring of Arc Welding for Quality and Defect Detection Mechanical Fastening Technologies for Steel to Aluminium Joining in Automotive Manufacture Process Capability Study for Friction Stir Spot Welding (FSSW) Resistance Spot Welding with Transition Discs – A Review of Dissimilar Joining Using Transition Materials with Specific Reference to Resistance Spot Welding Review of Process Simulations for Metal Additive Manufacturing Surface Modification and Micro-Machining with Pulsed-Laser Sources Wire Fed Electron Beam Additive Manufacture – A State-of-the-Art Review
 
Capabilities Banner
Innerpage Title Banner

TWI Technical Literature Review 30185

By Sullivan Smith

Background

To achieve ever more stringent fuel economy and performance targets the automotive sector has a need to dramatically reduce the weight of vehicles. Nearly all car manufacturers have a multi materials strategy, producing vehicles from a range of different steel grades and plastics, with more exotic aluminium, magnesium and composite components also becoming more common in mass produced cars. The main focus of this literature review is the case of steel to aluminium joining. At present no single technology exists that is able to join the full range of steel and aluminium panels that exist in a car body construction. But a wide range mechanical joining technologies have the potential to join certain combinations of steel and aluminium. The purpose of this literature review is to identify the technologies with the most potential for steel to aluminium joining and to assess their applicability for use in high volume car manufacture. This has been done by; examining material limitations, considering mulita sheet joint stacks, considering ease of robotisation, considering processing speed and cost and identifying any technique specific factors.

For more information please email:


contactus@twi.co.uk