Subscribe to our newsletter to receive the latest news and events from TWI:

Subscribe >
Skip to content

Guidance notes for Additive Manufacturing certification

The purpose of this document is to provide goal-based guidelines for the certification of metallic parts produced using an additive manufacturing (AM) process. The guidance is intended for those organisations that are:

  • interested in adopting AM and looking to understand how the qualification and certification requirements compare with conventional manufacturing processes;
  • already using AM and looking to qualify their processes or certify materials and/or parts;
  • sub-contracting, or intending to sub-contract, elements of their manufacturing to an AM supplier and wish to understand the requirements for certification.

Download your PDF