Innovative Linear Friction Welding Technology for Near Net Shape manufacture of advanced TI aerospace components

Innovative Linear Friction Welding Technology for Near Net Shape manufacture of advanced TI aerospace components

Acronym: TiFab
Funding body: Innovate UK
Status: Project

Rising material costs and the growing use of difficult-to-machine materials are spurring on designers to explore alternative, cheaper production methods. Near net shape forming technologies, which build parts instead of machining them from solid billets, potentially offer a range of benefits. The TiFab project aims to show how linear friction welding can be used to boost productivity of aerospace quality near net shape components for the airframe sector.