Low force mobile friction stir welding system for on-site marine fabrication
Acronym: Mobi-Weld
Funding body: European Commission
Status: Completed
The MobiWeld project will develop a prototype, mobile Friction Stir Welding (FSW) system, which will be designed and constructed for use in final fabrication/assembly in a shipyard environment.