Flexible fabrication of lightweight aluminium transport structures

Flexible fabrication of lightweight aluminium transport structures

Acronym: FlexiFab
Funding body: European Commission
Status: Completed

FlexiFab aims to create an automated robotic system to enable welding of aluminium components. The system will use friction stir welding technology (FSW). The welding method offers a number of benefits for aluminium joining/welding.