Which factors influence the sensitivity of a radiograph?

   

Frequently Asked Questions

The sensitivity of a radiograph is affected by contrast and definition. These are in turn influenced by the factors shown below.

factors that influence the sensitivity of a radiograph
factors that influence the sensitivity of a radiograph

For more information, please contact us.