Additive Manufacturing for Wear and Corrosion Applications

Additive Manufacturing for Wear and Corrosion Applications

Acronym: AMCOR
Funding body: European Commission
Status: Completed

"AMCOR will develop and demonstrate Laser Metal Deposition (LMD) industrial manufacturing systems for the deposition of functional graded coatings (FGM) and 3D features onto metallic components supplied by industry that are subjected to in-service wear and corrosion. This will be supported by the development, production and testing of mixed powder combinations for coatings suitability.