Thermally sprayed aluminium alloys for the prevention of corrosion and environmentally assisted cracking of welded corrosion resistant alloys
Status: Completed
Date Announced: April, 2006
Project reference: 16734
Fee £50,000. Completion date: December 2008<br/><br/><li>Welded 25Cr SDSS and 12Cr SMSS.<br/><li>TSA alloy compositions for control of polarisation to mitigate risk of HISC.<br/><li>Feasibility of internally protecting welds.<br/><li>TSA coatings under insulation of paint or aluminium foil.<br/>