Definition Of Sour Service Limits For Welded Type 316l And Cost Effective CRAs

Definition Of Sour Service Limits For Welded Type 316l And Cost Effective CRAs

Status: Completed
Date Announced: February, 2008
Project reference: 16170

Started July 2005. Cost per sponsor £50,000. Completion date June 2008. Project Leader: Briony Holmes. - Accurate sour service limits for 316L stainless steel defined - Summary of existing knowledge of SCC limits - Welded homogenous compared with welded metallurgically clad material - Ballot for changes to ISO 15156-3