Weldability Evaluation of Future Ultra Supercritical Power Plant Materials

Project Code: 0902-11

Objectives

Investigate the susceptibility of manufacturing cracking in IN740, IN617 and Haynes 230 by TIG and EB welding techniques

Compare the weldability of IN740, IN617 and Haynes 230 using selected filler metals

Project Outline

A number of test welds will be produced in TWI by TIG and EB welding techniques for IN740, IN617 and Haynes 230 using selected filler metals. The mechanical property, chemistry and microstructure of weldment and all-weld metal will be tested in room temperature and high temperature tensile and creep testing.

Relevant Industry Sectors

Power generation, Nuclear

Technical and Economic Benefits

A better understanding of the weldability of Ni base alloys for USC power plant application.

Providing a guidance to industry for the selection of welding technique and materials, including welding consumables for USC plants