Why are microwave-transparent adhesives important?

   

Frequently Asked Questions

An increasing number of electronic equipment applications require transmission or reception of a microwave signal. In many cases, these applications involve portable or mobile equipment where it is desirable to enclose the microwave antenna within the equipment's housing. Examples include mobile 'phone handsets, global positioning receivers and automotive collision-avoidance radar. In these applications, it is essential that the microwave signal is transmitted through the equipment housing, including any adhesive joints, without significant attenuation.