What is ''matching'' weld metal?

   

Weld metal which has a chemical composition and /or mechanical properties similar to that of the materials being joined. It does not mean that it has exactly the same characteristics; for instance, the corrosion performance of a matching weld metal almost always differs from that of the parent material.