The GG (Gimbal Gantry) Series FSW machine is the most versatile heavy section Friction Stir Welder on the market. It is capable of welding complex contours with agility only surpassed by a robot, but with power, precision and rigidity far superior to a robot.

These machines have been adopted by the high speed rail system manufacturers as the ultimate solution to welding complex train bodies on a massive scale. Not limited to the rail industry, these machines are also used by institutes of higher education and advanced material process research labs spanning the globe. Available in a fixed table or as an expandable rail version, these machines can be fit to the specific needs of any user in any market.

New MTI Weld process enhancing options include:

  • Friction Stir Welder-Gimbal Gantry StyleMTI FerrouStirT and IntelliStirT Closed-Loop Tool Temperature Control system adds superior temperature stability to the weld process resulting in unsurpassed weld quality and longer tool life while welding the most challenging to simplest range of weld material.
  • A Secondary weld head further increases weld efficiency and productivity by welding two sides of a panel at the same time.