Residual Stress Measurement Techniques for SLM Components

Back to Core Research Programme 34236-2023-literature-review-on-the-potential-use-of-non-destructive-testing-techniques-for-residual-stress-measurement 34241-2023-artificial-intelligence-for-ndt-scanning-of-unknown-geometries-using-collaborative-robots 34459-2022-friction-stir-welding-of-pressure-vessel-liners-for-the-storage-and-transportation-of-hydrogen 34727-2023-techniques-for-high-temperature-ultrasonic-inspection-of-arc-welding-state-of-the-art-review 34793-2023-update-on-literature-reviews-for-wire-fed-additive-manufacturing 34847-2023-Literature-review-on-crack-length-measurement-techniques-on-environmental-fracture-toughness-tests 35268-2024-Literature-review-on-dual-sensing-applications-for-SHM-of-pipelines 32221-2020-hybrid-composite-to-metal-joining 32893-2020-mechanical-fastener-coatings-for-corrosion-protection 33557-2020-extreme-high-speed-laser-application-ehla-coatings 33557-2020-extreme-high-speed-laser-application-ehla-coatings 33557-2020-extreme-high-speed-laser-application-ehla-coatings 33557-2020-review-of-electric-vehicle-battery-joining-methods-and-testing 34250-2022-thermoplastic-materials-compatibility-for-hydrogen-service A Review of High Power, In-Vacuum and Narrow Gap Laser Welding Processes for Thick Section Welding A Review of High Productivity Additive Manufacture Using a Hybrid Laser-Arc Deposition (HLAD) Process A Review of Micro Welding with Fibre and Disc Continuous-Wave Laser Sources A Review of Residual Stress Measurement Techniques Used for Components Produced Using the Selective Laser Melting Process A Review of the Machine GTAW Ambient Temperature Temper Bead Repair Technique for Nuclear Power Plant Components A Review of Weld Repairs of Mar-M247 and Similar Alloys Applications, Modelling and Manufacturing Processes for Perforated Composites - Literature Review Butt Fusion Welding Procedures and Test Methods Used for PE Pipes Duplex Stainless Steel Welding – A Review of Current Practices Elastic Follow-Up in the Context of Fracture Assessment Flaw Sizing Techniques Using Guided Waves Flaw Sizing Techniques Using Guided Waves Flaw Sizing Techniques Using Guided Waves In-Bore Multi-Positional Laser Welding In-Process Monitoring of Arc Welding for Quality and Defect Detection Mechanical Fastening Technologies for Steel to Aluminium Joining in Automotive Manufacture Process Capability Study for Friction Stir Spot Welding (FSSW) Resistance Spot Welding with Transition Discs – A Review of Dissimilar Joining Using Transition Materials with Specific Reference to Resistance Spot Welding Review of Process Simulations for Metal Additive Manufacturing Surface Modification and Micro-Machining with Pulsed-Laser Sources Wire Fed Electron Beam Additive Manufacture – A State-of-the-Art Review
 
Capabilities Banner
Innerpage Title Banner

TWI Technical Literature Review 22959

By R Fairclough

Background

A significant problem associated with components produced using the selective laser melting (SLM) process is the development of high internal residual stresses which are a result of the repeated heating and cooling of successive layers of powder during component build. This produces high temperature gradients and complex thermal effects within the build, which promote the development of significant residual stresses. If residual stresses are not recognised and allowed for in the design process for SLM manufactured parts, they can be a major factor in the subsequent failure of a component in service, particularly one subjected to alternating loadings or corrosive environments.

Residual stresses can also cause deformation in SLM manufactured parts which is problematic when tight dimensional tolerances are required. Often, some form of post processing (HIP or heat treatment) is required which can substantially increase manufacturing costs.