Reduced Pressure High Power Electron Beam Welding IP

What we do Banner
Innerpage Title Banner
Contact Us CTA

The difference between reduced pressure and conventional electron beam welding is primarily in the design of the electron gun. Novel gun design allows the process to be carried out at a rough vacuum level, or reduced atmospheric pressure, of around 1mbar compared with 10 -5 - 10 -2 mbar for conventional EBW. The technology was initially developed by Allan Sanderson at TWI in 1992 and has undergone continued development since this time.

A major benefit of the reduced pressure requirement is the ability to function with local seals or vacuum arrangements rather than a traditional vacuum chamber. Thus, large structures are now viable for EB welding.

Set-up and pump down times for RPEBW are up to 3 times quicker than conventional EBW allowing better utilisation of equipment and higher throughput. One further economic benefit is the lower capital purchase cost when compared to conventional EBW as a large chamber and high performance vacuum pumps are not required.

TWI has obtained patents for this technology in Europe, USA, Japan and a number of other countries (EP1018137, US6404115 & others).

The patents cover the method and equipment of RPEB, so anyone using the process needs permission (licence) from TWI.

TWI is pleased to offer non-exclusive licences to any potential users on reasonable commercial terms. Special arrangements are available for machine manufacturers, research institutes and universities.

For further information concerning licensing, please e-mail contactus@twi.co.uk.