Lead free: TWI prepares for new legislation


Connect, no.97, November/December 1998, p.6

c976cf1.jpg

The new millennium will see the implementation of environmental legislation which will ban a large number of materials, one of which is lead.

The development of new processes and materials will be essential by 2004. In preparation for this, TWI is undertaking a study on the wettability mechanisms for lead-free solders on lead-free metallised surfaces.

We are seeking the assistance of Member companies to supply components for analysis, in particular lead-free solder. Can you help?

For further information, please contact Sophie Lemort in the Advanced Materials and Processes Department. E-mail: slemort@twi.co.uk